Cracking paint can be caused by a variety of conditions ranging from the expansion and contraction of a substrate, moisture seepage problems or to something as simple as someone having applyed a water-base paint over an oil-base paint. 

 

First, try to determine what caused the cracking.  If, for instance, the problem is caused by the expanding and contracting of the painted material that is beyond your control, the problem will happen again and you should look for an alternative fix.  If the cracking occured because old caulk failed and allowed water into the substrate, you can simply recaulk after your paint job is complete to eliminate future problems.  Knowing why something happened can prevent having to re-do a job several times.

 

Materials Needed

 

Scraper, sandpaper, primer, paint, putty knife, spackling compound

 

Steps

 

  1. Scrape the substrate with a scraper to remove all loose or flaking paint.
  2. Lightly feather sand the edges of the paint you scraped off to make the surface smooth.
  3. Using a putty knife, apply a skim coat of spacking to fill in cracks and level out the surface.
  4. Prime the area that was patched with a primer.
  5. Apply two coats of finish coat paint.

 


Related Items:

How To Paint Ceramic Tile
How To Paint Kitchen Cabinets
How To Waterproof A Basement Wall
How To Stain A Deck
How To Strip Paint and Stain
How To Stop Peeling Paint
Which Primer Should I Use?
 

 

Partner Websites

Want Your Link Here?

Contact Us To be added as a partner on this page.


How2Instructions.com and its owners are in no way liable for any problems, frustrations or damages that may result from following instructions listed here.

This website is purely for informational purposes and all projects are done at your own risk.

 

© 2008 How2Instructions.com
 
Joomla Template by Joomlashack | WebSite Design by North Coast Designs
Joomla Templates by JoomlaShack Joomla Templates